AWS A5.4 E309-16 Ibikoresho byo gusudira ibyuma bya elegitoronike yo gusudira ibikoresho byo gusudira, ibikoresho byo gusudira

Ibisobanuro bigufi:

A302 (AWS E309-16) ni Cr23Ni13 electrode idafite ibyuma idafite titanium-calcium.


Ibicuruzwa birambuye

Ibicuruzwa

Ibyuma byo gusudira ibyuma

A302                                      

GB / T E309-16

AWS A5.4 E309-16

Ibisobanuro: A302 ni Cr23Ni13 ibyuma bitagira umuyonga electrode hamwe na titanium-calcium.Irashobora gukoreshwa kuri AC na DC hamwe nibikorwa byiza byo gukora.Icyuma cyabitswe gifite imbaraga nyinshi zo kurwanya no kurwanya okiside.

Gushyira mu bikorwa: Ikoreshwa mu gusudira ubwoko bumwe bwibyuma bidafite ingese, ibyuma bidafite ingese, ibyuma bidasanzwe (Cr19Ni9 ni kimwe nicyuma gito cya karubone), ibyuma bya chromium ndende, ibyuma bya manganese, nibindi.

 

Ibigize imiti yicyuma (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

.080.08

0.5 ~ 2.5

90.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

.040.040

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Kurambura

%

Bijejwe

50550

≥25

 

Icyifuzo kigezweho:

Diameter

(Mm)

2.5

3.2

4.0

5.0

Kuzenguruka

A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha 1 kuri 150 ℃ mbere yo gusudira;

2. Kuberako ubujyakuzimu bwinjira ari buke mugihe cyo gusudira AC, amashanyarazi ya DC agomba gukoreshwa uko bishoboka kwose kugirango yinjire cyane.kandi ikigezweho ntigikwiye kuba kinini kugirango wirinde gutukura inkoni yo gusudira.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka isaga 20 dukora umwuga wo gukora electrode yo gusudira, inkoni zo gusudira, hamwe n’ibikoresho byo gusudira.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.