Electrode yo gusudira mu byuma bitagira umwanda
A022
GB/T E316L-16
AWS E316L-16
Ibisobanuro: A022 ni electrode y'icyuma kitagira umuvuduko wa karuboni Cr18Ni12Mo2 ifite karuboni nkeya cyane ifite igipfundikizo cya titanium calcium. Ishobora gukoreshwa haba kuri AC na DC ifite imikorere myiza. Ingano ya karuboni mu cyuma cyashyizwemo ni ≤0.04%, ibi biyiha ubushobozi bwo kurwanya ubushyuhe, kurwanya ingese no kurwanya imiyoboro.
Ikoreshwa: Ikoreshwa mu gusudira urea, fibre y’ubukorikori n’ibindi bikoresho ndetse n’ubwoko bumwe bw’icyuma kitagira umugese. Ishobora kandi gukoreshwa mu byuma bitagira umugese bya chromium, ibyuma bivanze n’ibyuma bitandukanye bidashobora kuvurwa ubushyuhe nyuma yo gusudira.
Imiterere ya shimi y'icyuma gisukwa (%):
| C | Mn | Si | Cr | Ni | Mo | Cu | S | P |
| ≤0.04 | 0.5 ~ 2.5 | ≤0.90 | 17.0 ~ 20.0 | 11.0 ~ 14.0 | 2.0 ~ 3.0 | ≤0.75 | ≤0.030 | ≤0.040 |
Imiterere ya tekiniki y'icyuma gisudira:
| Ikintu cyo kugerageza | Imbaraga zo gukurura Mpa | Kurekura % |
| Yemejwe | ≥490 | ≥30 |
Ikoreshwa ry'amashanyarazi risabwa:
| Umwanya w'inkoni (mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 |
| Umuyoboro wo gusudira (A) | 25 ~ 50 | 50 ~ 80 | 80 ~ 110 | 110 ~ 160 | 160 ~ 200 |
Itangazo:
1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 150°C mbere yo gusudira;
2. Kubera ko ubujyakuzimu bw'amazi buto cyane mu gihe cyo gusudira AC, ingufu za DC zigomba gukoreshwa uko bishoboka kose kugira ngo zigere ku buryo bwimbitse. Kandi umuriro ntugomba kuba munini cyane kugira ngo wirinde gutukura kw'icyuma gisudira;
3. Ubudahangarwa bw'icyuma cyabitswe buterwa n'ubwumvikane bubiri bw'ibitangwa n'ibikenewe.
Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka irenga 20 dukora electrodes zo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.
Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.