Ubwiza Bwiza bwa Tyue Brand AWS A5.11 ENiCu-7 Nickel ishingiye kuri Welding Electrode, Nickel Alloy Welding Rods yo gusudira Arc

Ibisobanuro bigufi:


Ibicuruzwa birambuye

Ibicuruzwa

Nickel na Nickel Alloy Welding Electrode

Ni207                                                     

GB / T ENi4060

AWS A5.11 ENiCu-7

Ibisobanuro: Ni207 ni Monel alloy electrode hamwe na sodium ya hydrogène nkeya.Koresha DCEP (itaziguye ya electrode nziza) kandi ifite imikorere myiza yo gusudira no guhangana.

Gusaba: Kubisudira Monel cyangwa ibyuma bidasa.Irashobora kandi gukoreshwa murwego rwo hejuru rwo gusudira inzibacyuho.

 

Ibigize imiti yicyuma (%):

C

Mn

Fe

Si

Al

Ti

Cu

Nb

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤1.0

≤1.0

27.0 ~ 34.0

≤2.5

≥62.0

≤0.015

≤0.020

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Bijejwe

80480

≥200

≥27

 

Icyifuzo kigezweho:

Diameter

(Mm)

3.2

4.0

Umuyoboro wo gusudira

A)

90 ~ 110

110 ~ 150

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha 2 hafi 300 ℃ mbere yo gusudira;

2. Ni ngombwa guhanagura ingese, amavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira.Gerageza gukoresha arc ngufi kugirango usudire.

 