Electrode za ENiCrFe-3 za Nickel

Ibisobanuro bigufi:

Electrode irimo gushyiramo icyuma cya 65Ni-20Cr-2Nb-1.5Mo.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

KODE YA ISO YA EN: 14172: ENi6082

Electrode irimo gushyiramo icyuma cya 65Ni-20Cr-2Nb-1.5Mo. Icyuma cya X-ray gifite imiterere myiza cyane. Kirakwiriye cyane mu gusudira alloys zifite imiterere isa nayo, ku byuma bifite Nickel-Chromium-Iron alloy iyo ingano ya Manganese nyinshi ntacyo yangiza, ku byuma bya Nickel Chromium-Iron bivanze na Nickel hamwe n'ibyuma bitandukanye. Kirakwiriye gupfuka ibyuma bya forge. Cyane cyane mu gusudira 9% Ni Steels kugira ngo ikoreshwe mu gusudira. Kinakoreshwa mu gusudira alloys za Nickel-Chromium zikoreshwa mu bushyuhe bwinshi nko gushyushya itanura n'imiyoboro ya reformer.

IKIMENYETSO CY’UBUTASI CY’IBYUMA BYOSE BYO GUSHUSHANYA

Igice C Mn Si Cr Ni Fe Nb Cu Ti S P
Ijanisha ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

IMITERERE ISANZWE Y'IBYUMA BYOSE BYO GUSHUSHANYA

UTS YS Kurekura Imbaraga z'ingaruka za CVN (J) Kwaguka kw'impande Imbaraga zo gutera
(MPa) (MPa) (L= 5d)% kuri Nomero 196°C kuri 196°C (mm) 600°C mu gihe cy'amasaha 1000.
620 500 30 75 0.85 160 MPa

AMAKURU Y'IBYIHUTIRWA N'AYO GUPAKIRA: DC (+)

Ingano (mm)

Uburebure bwa Dia x

5×350

4×350

3.15×350

2.5×350

Ingano y'Ubu (Amps)

150-180

120-150

80-110

60-70

Uburemere/Ikarito (kgs)

2.5

2.5

2.5

2.5

Kwitonda

1. Menya neza ko electrode zumutse. Ongera wumishe electrode kuri dogere selisiyusi 300-325 mu gihe cy'isaha imwe.

2. Komeza ugire umugozi mugufi, ushyireho umugozi kandi ugabanye ubushyuhe buvamo.

3. Reka ubushyuhe bukonje kugeza munsi ya 50 C mbere yo gushyiramo, hanyuma ushyireho urwego rukurikiraho.