Electrode y'icyuma cya TYUE E308-16

Ibisobanuro bigufi:

Electrode yo gusudira yo mu bwoko bwa titaniyumu ikoreshwa mu byuma bidakoresha karuboni nyinshi.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Ishyirwa mu byiciro:

AWS A5.4 / ASME SFA5.4 E308-16

JIS Z3221 D308-16

Ibisobanuro:

Electrode yo gusudira mu byuma bitagira umwandaE308-16 ni ubwoko bwa titaniyumuelectrode yo gusudiraku byuma bidashonga cyane bifite karuboni nkeya. Icyuma gikoreshwa mu gusudira gifite ubushobozi bwiza bwo kurwanya ingese hagati y’udusimba bitewe n’uko karuboni irimo ari ≤. 0.04% b. Gishobora gukoreshwa mu gusudira ahantu hose hamwe n’imikorere myiza: umurambararo uhamye, uduce duto, imiterere myiza ya sudde. Kandi no muelectrode yo gusudiraigaragaza ubushobozi bwo kwirinda ubushyuhe, ntabwo byoroshye guhindura umutuku kandi nta myenge ya gaze iboneka.

Porogaramu:

Gusudira by'icyuma cya 18%Cr-8%Ni.

Ikwiriye inyubako zo gusudira zakozwe mu cyuma kitagira umukungugu cya 022Cr-19Ni10, nk'imigozi y'ubukorikori, ifumbire,

ibikoresho bya peteroli, nibindi.

Ibigize imiti mu byuma byabitswe (E308L-16) (%)

Ikintu C Mn Si Cr Ni S P Cu Mo
agaciro gasanzwe ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
Agaciro k'urugero 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

Imiterere ya tekiniki y'ibyuma byabitswe (%)

Imikorere yo kurwanya ingese n'imiterere ya ferrite bigomba kugenwa hagati y'umuguzi n'umugurisha.

Ikintu Imbaraga zo Gukurura (MPa) Uburebure (%)
agaciro gasanzwe ≥550 ≥25
Agaciro k'urugero 601 41

Ingano (mm)

2.0

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira (A)

25-50

50-80

80-110

110-160

160-200

 

Ibisobanuro ku ikoreshwa:

1. Komeza umugozi ube mugufi uko bishoboka kose.

2. Kuraho imyanda nk'amavuta n'umukungugu mu mwobo.

3. Shyira electrodes kuri dogere 350 (662) mu gihe cy'iminota 60 mbere yo kuyikoresha


  • Ibanjirije iyi:
  • Ibikurikira: