Ibisobanuro bigufi:

Ubu ni electrode itandukanye yo gusudira kugirango igaragare hejuru yo gusudira ibyuma bya karubone cyangwa ibyuma bivangavanze hamwe na valve hamwe nubushyuhe bwakazi buri munsi ya 450 ° C.


Ibicuruzwa birambuye

Ibicuruzwa

UKORESHE:

Ubu ni electrode itandukanye yo gusudira kugirango igaragare hejuru yo gusudira ibyuma bya karubone cyangwa ibyuma bivangavanze hamwe na valve hamwe nubushyuhe bwakazi buri munsi ya 450 ° C.

BIKURIKIRA METAL CHIMICAL COMPOSITION (%):

C

Cr

S

P

Ibindi bintu byose hamwe

agaciro k'ingwate

≤0.15

10.00 ~ 16.00

≤0.030

.040.040

≤2.50

Urugero agaciro

0.13

13.34

0.006

0.022

-

GUKURIKIRA UMUYOBOZI:

(Umuyaga ukonje nyuma yo gusudira) HRC ≥ 40

AKARERE KA BIKORWA (DC +):

Diameter ya electrode (mm)

φ3.2

φ4.0

φ5.0

Umuyoboro wo gusudira (A)

80 ~ 120

120 ~ 160

160 ~ 200

IMYITOZO:

⒈ gusudira electrode kuba 300 ~ 350 ℃ guteka 1h.

⒉ mbere yo gusudira igihangano kugirango gishyushye kugeza 300 ℃ hejuru, nyuma yo gusudira imiti itandukanye irashobora kubona ubukana bukwiye.

WELDING RODS AWS E6010:

AWS E6010 ni ubwoko bwa selile-Na ubwoko bwo gusudira electrode, idasanzwe kuri DC.Ifashisha ikoranabuhanga ryateye imbere ryamahanga, rifite ARC ryimbitse cyane, uduce duke, gutandukana byoroshye, gusudira cyane, gukora neza.Irashobora gukoreshwa mu gusudira kumwanya wose, guhagarikwa hejuru no kumanuka umwanya wo gusudira nibindi birashobora kugera ku ngaruka uruhande rumwe rusudira impande zombi.

GUSABA:

Inkoni yo gusudira AWS E6010 cyane cyane yo gusudira umuyoboro wibyuma bya karubone cyangwa ibikoresho bimwe, gusubiza inyuma gusudira / kuzuza weld / kwisiga gusudira kumiterere yicyuma hepfo.

Ibigize imiti (%)

UMUTUNGO W'IKORANABUHANGA W'UBURYO BWA DEPOSITED:

Ikizamini Rm (N / mm2) Rel (N / mm2) A (%) KV2 (J) 0 ℃
Agaciro k'ingwate 60460 40340 ≥16 ≥47
Igisubizo rusange 485 380 28.5 86

AKARERE KA (DC):

Diameter φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

ICYITONDERWA:

1. Biroroshye guhura nubushuhe, nyamuneka ubigumane neza.

2. Irakeneye gushyuha mugihe ipaki yamenetse cyangwa ubushuhe bwakiriwe, ubushyuhe bwo gushyushya bugomba kuba hagati ya 70C kugeza 80C, igihe cyo gushyushya kigomba kuva kuri 0.5 kugeza kumasaha 1.

3. Iyo ukoresheje electrode yo gusudira 5.0mm, nibyiza gukoresha imbaraga-zohejuru, nkeya-nkeya, kugirango uzamure imikorere yo gusudira.

C Mn Si S. P
<0.2 0.3-0.6 <0.2 <0.035 <0.04