Gusudira mu byuma bitagira umwandaElectrode
A042
GB/T E309MoL-16
AWS E309MoL-16
Ibisobanuro: A042 ni electrode y'icyuma kitagira umugese ya Cr23Ni13Mo2 ifite karubone nkeya cyane ifite titanium calcium coat. Ishobora gukoreshwa haba kuri AC na DC. Bitewe no kongeramo ingano ikwiye ya molybdenum, ubushobozi bwo kudacika no kudacika kw'icyuma cyashyizwemo burushaho kwiyongera.
Ikoreshwa: Ku bwoko bumwe bw'ibikoresho by'icyuma kitagira umukungugu bikozwe mu buryo bwa ultra-low carbon (nk'umunara wa synthesis urea) n'ibindi bisa nabyo.
Imiterere ya shimi y'icyuma gisukwa (%):
| C | Mn | Si | Cr | Ni | Mo | Cu | S | P |
| ≤0.04 | 0.5 ~ 2.5 | ≤0.90 | 22.0 ~ 25.0 | 12.0 ~ 14.0 | 2.0 ~ 3.0 | ≤0.75 | ≤0.030 | ≤0.040 |
Imiterere ya tekiniki y'icyuma gisudira:
| Ikintu cyo kugerageza | Imbaraga zo gukurura Mpa | Kurekura % |
| Yemejwe | ≥520 | ≥25 |
Ikoreshwa ry'amashanyarazi risabwa:
| Umwanya w'inkoni (mm) | 2.5 | 3.2 | 4.0 | 5.0 |
| Umuyoboro wo gusudira (A) | 50 ~ 80 | 80 ~ 110 | 110 ~ 160 | 160 ~ 200 |
Itangazo:
1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 150°C mbere yo gusudira;
2. Kubera ko ubujyakuzimu bw'amazi buto cyane mu gihe cyo gusudira AC, ingufu za DC zigomba gukoreshwa uko bishoboka kose kugira ngo zigere ku buryo bwimbitse. Kandi umuriro ntugomba kuba munini cyane kugira ngo wirinde gutukura kw'icyuma gisudira;
3. Ubudahangarwa bw'icyuma cyabitswe buterwa n'ubwumvikane bubiri bw'ibitangwa n'ibikenewe.
Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, naibikoresho byo gusudiraimyaka irenga 20.
Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.