Inkoni zo gusudira za AWS E6011

Ibisobanuro bigufi:

Electrode yo gusudira ya AWS E6011 ni ubwoko bwa potasiyumu ya selulosi, ikoreshwa mu gusudira ihagaze. Haba mu gusudira AC na DC.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

AWS E6011electrode yo gusudirani ubwoko bwa potasiyumu ya selulosi, ikoreshwa mu gusudira iburyo. Haba mu gusudira AC na DC. Ikoresha ikoranabuhanga rigezweho ryo mu mahanga kandi ifite imiterere myiza y'ikoranabuhanga ryo gusudira. Uburebure bwa ARC bugomba kugenzurwa mu rugero rukwiye. Ntabwo ari isudira ikwiye kandi ipfundikiye.

Porogaramu

Inkoni zo gusudira AWS E6011 zikwiriye inyubako z'amato zo gusudira nk'inyubako n'ibiraro, ibigega byo kubikamo ibintu, imiyoboro n'ibikoresho by'amato byo gusudira.

IBIKORESHO:

Gutangiza vuba vuba

Inzira yo hejuru y'umusemburo

Ibisigazwa by'ibishishwa bivamo byoroshye

Igikorwa cyiza cyo kunyobwa. IBYIZA:

Guteranya umugozi byoroshye, ni byiza cyane mu gufataho udupfundikizo

Uburyo bwiza bwo kwinjira

Gusukura vuba

Kugaragara neza kw'amasaro, bigabanya ubukonje n'igabanuka ry'umubyimba

UBWOKO BW'UMURIRO: Electrode y'umuriro igororotse (DCEP) cyangwa AC

UBUHANGA BWO KUSURISHA BUSUKURA BWITEGANYA:

Uburebure bw'Umurongo - Uburebure mpuzandengo (1/8” kugeza 1/4”)

Igorofa - Komera imbere y'ikidendezi kandi ukoreshe uburyo bwo gukubita buhoro

Electrode y'inguni igororotse - Ifite inguni gato igana hejuru y'ikibaho

Uhagaze Hejuru - Uburyo bwo gukubita cyangwa kuboha gato

Guhagarara Uhagaze - Koresha imbaraga nyinshi kandi wihuta mu rugendo, ukomeze imbere y'ikidendezi

Hejuru - Komeza imbere y'ikidendezi kandi ukoreshe uburyo bwo gukubita buhoro

Ibikubiye mu binyabutabire (%)

C Mn Si S P
<0.12 0.3-0.6 <0.2 <0.035 <0.04

Imiterere ya tekiniki y'ibyuma byabitswe

Ikintu cy'igerageza

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0℃

Agaciro k'ingwate

≥460

≥330

≥16

≥47

Ibisubizo Rusange

485

380

28.5

86

Ikoreshwa ry'Umuyoboro w'Ifatizo (DC)

Ingano

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40 ~ 70

50 ~ 90

90 ~ 130

130 ~ 210

170 ~ 230

Icyitonderwa:

1. Biroroshye kubishyira ahantu hafite ubushuhe, nyamuneka bigumishe ahantu humutse.

2. Ikeneye gushyushya iyo ipaki yangiritse cyangwa ubushuhe buyinjijwemo, ubushyuhe bwo gushyushya bugomba kuba hagati ya 70C na 80C, igihe cyo gushyushya kigomba kuba kuva kuri 0.5 kugeza ku isaha 1.

3. Mu gihe ukoresha electrode zo gusudira za 5.0mm, ni byiza gukoresha amashanyarazi menshi kandi make, kugira ngo wongere imikorere yo gusudira.