AWS E7015-A1 Ubushyuhe-butarwanya ibyuma bya electrode R107 Amashanyarazi make ya hydrogene yo gusudira Inkoni ya Electrode

Ibisobanuro bigufi:

R107 (AWS E7015-A1) ni electrode ya pearlitike irwanya ubushyuhe hamwe na sodium ya hydrogène nkeya irimo 0.5% Mo.


Ibicuruzwa birambuye

Ibicuruzwa

Molybdenum na Chromium Molybdenum Ubushyuhe bwo Kurwanya IbyumaGusudiraElectrode

R107                                                     

GB / T E5015-A1

AWS A5.5 E7015-A1

Ibisobanuro: R107 ni pearlitike yubushyuhe bwumuriro wa electrode hamwe na sodium ya hydrogène nkeya irimo 0.5% Mo. Koresha DCEP (electrode itaziguye) kandi irashobora gusudira mumyanya yose. Gusudira bigomba gushyuha kugeza 90 ~ 110 ℃ mbere yo gusudira. .

Gushyira mu bikorwa: Irakoreshwa mu gusudira imiyoboro itetse ifite ubushyuhe bwo gukora munsi ya 510 ° C (nka 15Mo, nibindi), kandi irashobora no gukoreshwa mu gusudira muri rusange ibyuma bito bito-bikomeye cyane.

 

Ibigize imiti yicyuma (%):

C

Mn

Si

Mo

S

P

≤0.12

0.50 ~ 0.90

≤0.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Agaciro k'ingaruka (J)

Ubushuhe busanzwe.

Bijejwe

90490

90390

≥22

≥47

 

Diffusion hydrogène yibikoresho byabitswe: ≤6.0mL / 100g (uburyo bwa glycerine)

Igenzura rya X-ray: I amanota

 

Icyifuzo kigezweho:

Diameter

(Mm)

2.0

2.5

3.2

4.0

5.0

GusudiraIbiriho

A)

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha 1 kuri 350 ℃ mbere yo gusudira;

2. Ni ngombwa guhanagura ingese, igipimo cyamavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira.