AWS E7016-A1 Imashini zo gusudira zirwanya ubushyuhe R106 Molybdenum na Chromium Molybdenum

Ibisobanuro bigufi:

R106 (AWS E7016-A1) ni electrode y'icyuma irinda ubushyuhe ifite igishishwa gito cya hydrogen potasiyumu kirimo 0.5% Mo.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Molybdenum na Chromium Molybdenum Molybdenum Electrode yo gusudira icyuma idashyuha

R106                                                     

GB/T E5016-A1

AWS A5.5 E7016-A1

Ibisobanuro: R106 ni electrode y'icyuma irinda ubushyuhe ifite igishishwa cya potasiyumu nkeya irimo 0.5% Mo. Ishobora gukoreshwa mu gusudira ahantu hose hamwe na AC na DC. Gusudira bigomba gushyuha kugeza kuri 90 ~ 110 ℃ mbere yo gusudira.

Ikoreshwa: Ikoreshwa mu gusudira imiyoboro ya boiler ifite ubushyuhe buri munsi ya 510°C, nk'imiyoboro ya 15Mo, AST-MA204 na A335-P1, n'ibindi. Ishobora kandi gukoreshwa mu gusudira ibyuma binini bifite imbaraga nkeya.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Mo

S

P

≤0. 12

≤0.60

≤0.40

0.40 ~ 0.65

≤0.030

≤0.030

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Agaciro k'ingaruka (J)

Ubushyuhe Busanzwe.

Yemejwe

≥490

≥390

≥20

—

Byapimwe

530

420

27

60

 

Isuzuma rya X-ray: Icyiciro cya mbere

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni (mm)

2.5

3.2

4.0

Umuyoboro wo gusudira (A)

Gusudira mu buryo burambuye

80 ~ 110

110 ~ 140

170 ~ 200

Gusudira mu buryo buhagaze,

Gusudira hejuru

70 ~ 90

100 ~ 120

140 ~ 170

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe kuri 150 ~ 200℃ mbere yo gusudira;

2. Ni ngombwa gusukura ingese, ibipimo by'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira.