Ama-electrode yo gusudira ya AWS E312-16 mu byuma bitagira umugese, Electrode zo gusudira mu byuma bikozwe mu manual, Solder

Ibisobanuro bigufi:

AFE312-16 (AWS E312-16) ni electrode y'icyuma kitagira umugese ya Cr29Ni9 ifite irangi rya titaniyumu na kalisiyumu.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira mu byuma bitagira umwanda

AF312-16

GB/T E312-16

AWS A5.4 E312-16

Ibisobanuro: AFE312-16 ni electrode y'icyuma kitagira umugese ya Cr29Ni9 ifite titanium-calcium coating. Ishobora gukoreshwa haba kuri AC na DC ifite imikorere myiza. Kubera ko irimo molybdenum na azote, kandi ingano ya karuboni ikaba nke cyane, icyuma cyashyizwemo gifite ubushobozi bwo kurwanya imyakura no kurwanya ingese, cyane cyane kurwanya ingese.

Ikoreshwa: Ikoreshwa mu gusudira ibyuma 29-9 by'uruhererekane bya stainless steel, ibyuma bikozwe mu cyuma n'ibindi bisa, ndetse no gusudira ibikoresho bishobora kwangirika no gupfunyika.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.15

0.5 ~ 2.5

≤0.90

28.0 ~ 32.0

8.0 ~ 10.5

≤0.75

≤0.75

≤0.030

≤0.040

 

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

 Imbaraga zo gukurura

Mpa

Kurekura

%

Yemejwe

≥660

≥22

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(cyangwa semm)

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(cyangwa seA)

50 ~ 80

80 ~ 110

100 ~ 150

140 ~ 180

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 250°C mbere yo gusudira.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka irenga 20 dukora electrodes zo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 


  • Ibanjirije iyi:
  • Ibikurikira: