E308L-17 Icyuma gishyushya gikozwe mu byuma bitagira umugese

Ibisobanuro bigufi:

E308L-17 yo Gusudira Icyuma Gitarangwamo Ingufu zo Gusudira (C yo hasi, 18%Cr- 8%Ni)


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

E308L-17 yo Gusudira Icyuma Gitarangwamo Ingufu zo Gusudira (C yo hasi, 18%Cr- 8%Ni)

Gushyira mu byiciro

EN IS03581-A: 2016: E 19 9 L R 12

EN IS03581-B: 2016: ES308L-17

AWS A5.4-2014: E308L-17

JISZ 3221-2013: ES308L-17

Ibisobanuro

-Gupfuka ni ubwoko bwa titania y'ishwagara mu gusudira icyuma kitagira umugese cya 18%Cr-8%Ni. (AISI 301, 302, 304, 308)

-Ubuhanga bwiza bwo gusudira kubera ko ifite igipimo cyo hejuru cyo gushyiramo.

-Kura amazi, ingese, amavuta n'ibindi bintu byose by'inyuma mu mwobo mbere yo gusudira.

-Ikoreshwa neza hamwe n'ibikoresho bikoresha umuriro w'amashanyarazi.

-Gushyushya mbere ntabwo ari ngombwa muri rusange.

-Sukura electrode kuri 250 ~ 350 °C mu gihe cy'iminota 30 ~ 60 mbere yo kuyikoresha.

Ibigize imiti mu byuma byabitswe (%)
C Mn Si Cr Ni S P Mo Cu Fn
0.03 0.65 0.73 18.95 9.82 0.012 0.028 0.21 0.30 6.4

 

Ingano n'Ingufu zisabwa (AC cyangwa DC)
Umwanya w'inkoni yo gusudira
(mm)
2.5 3.2 4.0 5.0
umuyoboro wo gusudira
(A)
55-80 90-130 110-150 140-180

Ibiranga Imikoreshereze:

Umuheto uhamye cyane.

Gukuraho neza cyane ibisigazwa by'imyanda.

Kwinjira ni gake cyane.

Ubudahangarwa bwiza bw'ubushyuhe n'ingese.

Ubudahangarwa bwiza cyane bw'imipfundo.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka 22 dukora ibikoresho byo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira ibyuma bito, electrode zo gusudira hejuru, electrode zo gusudira za nikeli na kobalti, insinga zo gusudira ibyuma bito n'ibito, insinga zo gusudira ibyuma bidashonga, insinga zikingira gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nikeli na kobalti, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira..


  • Ibanjirije iyi:
  • Ibikurikira: