ERCuSn-A (Phos Bronze A) Umuringa n'umuringa Alloy Bare Rods na Electrodes Tig na Mig Wire

Ibisobanuro bigufi:

ERCuSn-A Phos Bronze A ni umuringa wa zinc-zinc urimo amabati agera kuri 5% na fosifore igera kuri 0.35% yongeweho nka deoxidizer ikoreshwa mu gusudira umuringa n'umuringa.


Ibicuruzwa birambuye

Ibicuruzwa

ERCuSn-A Phos Bronze A ni umuringa wa zinc-zinc urimo amabati agera kuri 5% na fosifore igera kuri 0.35% yongeweho nka deoxidizer ikoreshwa mu gusudira umuringa n'umuringa.Irashobora kandi gukoreshwa mu gusudira umuringa niba kuba amabati mu cyuma gisudira bitemewe.

Porogaramu isanzwe: gutwikira ibyuma;guhuza 509-519 urukurikirane rwa tin-bronze ibyuma fatizo

Icyiciro cya AWS: ERCuSn-A Icyemezo: AWS A5.7 / A5.7M: 2007
Amavuta: ERCuSn-A ASME SFA A5.7

 

Umwanya wo gusudira: Ibiriho:
AC-DCEP

 

Imbaraga za Tensile, kpsi: 35
Brinell Gukomera 70-85

Ububiko busanzwe bwa chimie nkuko AWS A5.7 (indangagaciro imwe ni ntarengwa)

Cu harimo Ag Al Pb P Sn Ibindi
Ibisigaye 0.01 0.02 0.10-0.35 4.0-6.0 0.50

 

Ibipimo bisanzwe byo gusudira
Diameter Inzira Volt Amps GAS
in (mm)
1/16 (1.6) GTAW 70-120 70-150 ACHF ukoresheje 100% Argon cyangwa Helium 2% Thoriated, Ceriated cyangwa Lanthanum Tungsten Electrode
3/32 (2.4) GTAW 120-160 140-230 ACHF ukoresheje 100% Argon cyangwa Helium 2% Thoriated, Ceriated cyangwa Lanthanum Tungsten Electrode
1/8 (3.2) GTAW 170-230 225-320 ACHF ukoresheje 100% Argon cyangwa Helium 2% Thoriated, Ceriated cyangwa Lanthanum Tungsten Electrode
Ibipimo bisanzwe byo gusudira
Diameter Inzira Volt Amps GAS
in (mm)
0.035 (1.6) GMAW 20-26 100-200 100% Argon cyangwa 75% Argon, 25% Helium
0.045 (2.4) GMAW 22-28 100-250 100% Argon cyangwa 75% Argon, 25% Helium
1/16 (3.2) GMAW 29-32 250-400 100% Argon cyangwa 75% argon, 25% Helium
3/32 (3.2) GMAW 32-34 350-500 100% Argon cyangwa 75% Argon, 25% Helium

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka isaga 20 dukora umwuga wo gukora electrode yo gusudira, inkoni zo gusudira, hamwe n’ibikoresho byo gusudira.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.

 

 

 

 


  • Mbere:
  • Ibikurikira: