RBCuZn-B (Nickel Bronze) Brazing Filler Ibyuma byo gusudira

Ibisobanuro bigufi:

RBCuZn-B Nickel Bronze (RBCuZn-B) ibyuma byuzuza ibyuma bisa n'umuringa wo mu mazi ariko birimo manganese na fer byongera ubukana n'imbaraga zo kubitsa weld.


Ibicuruzwa birambuye

Ibicuruzwa

RBCuZn-B Nickel Bronze (RBCuZn-B) ibyuma byuzuza ibyuma bisa n'umuringa wo mu mazi ariko birimo manganese na fer byongera ubukana n'imbaraga zo kubitsa weld.Harimo kandi nikel yemeza gukwirakwiza icyuma mububiko.Ikirimi kitagira aho kibogamiye cyangwa gike ya okiside na acide ya boric / ubwoko bwa flux.

Icyiciro cya AWS: RBCuZn-B Icyemezo: AWS A5.8 / A5.8M: 2011
Amavuta: RBCuZn-B ASME SFA A5.8

 

Umwanya wa Brazing: H, V. Urubuga rwa Brazing:
1620-1800⁰F

 

Imbaraga za Tensile, kpsi: 60-78
Kurambura%, min: 25

 

Ingingo yo gushonga 1620⁰F Gukomera 1590⁰F Brinell Gukomera 80-110

Ububiko busanzwe bwa chimie nkuko AWS A5.8 (indangagaciro imwe ni ntarengwa)

Cu Zn Sn Fe Mn Ni Pb Al Si Ibindi
56.0-60.0 Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0.50

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka isaga 20 dukora umwuga wo gukora electrode yo gusudira, inkoni zo gusudira, hamwe n’ibikoresho byo gusudira.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.

 

 

 

 


  • Mbere:
  • Ibikurikira: