J607 (AWS E9015-D1) Electrode zo gusudira z'icyuma gito cya Alloy Electrode z'icyuma gikomeye cyane

Ibisobanuro bigufi:

J607 (AWS E9015-D1) ni electrode y'icyuma ifite imbaraga nkeya kandi idafite hydrogen sodium nyinshi.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Icyuma gito cya AluminiyumuGusudiraElectrode

J607                                       

GB/T E6015-D1

AWS E9015-D1 

 

Ibisobanuro: J607 ni electrode y'icyuma ifite imbaraga nkeya ifite igishishwa cya sodium nkeya ya hydrogen. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse), kandi ishobora gusukurwa ahantu hose.

Ikoreshwa: Ikoreshwa mu gusudira ibyuma bipima karuboni n'ibyuma bifite imbaraga nkeya bifite imbaraga zijyanye nabyo, nka Q420, nibindi.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Agaciro k'ingaruka (J)

-30℃

Yemejwe

≥590

≥490

≥15

≥27

Byapimwe

620 ~ 680

≥500

20 ~ 28

≥27

 

Ingano ya hydrogen mu byuma byabitswe: ≤4.0mL/100g (uburyo bwa glycerin) 

Isuzuma rya X-ray: Icyiciro cya mbere

 

Ikoreshwa ry'amashanyarazi risabwa:

(mm)

Umwanya w'inkoni

2.0

2.5

3.2

4.0

5.0

5.8

(A)

GusudiraUbu

60 ~ 80

70 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

210 ~ 260

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe kuri dogere 350 mbere yo gusudira;

2. Ni ngombwa gusukura ingese, igipimo cy'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira;

3. Koresha uburyo bwo gusudira bugufi mu gihe usuka. Uburyo bwo gusudira buto bukwiye.


  • Ibanjirije iyi:
  • Ibikurikira: