Ibisobanuro bigufi:

ERCuSn-A Phos Bronze A ni umuringa-zinc ugizwe na tin ingana na 5% na fosifore ingana na 0.35% yongerwamo nk'icyuma gikoreshwa mu gusudira umuringa n'umuringa.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

RBCuZn-A Naval Bronze (RBCuZn-A) ni icyuma gikozwe mu muringa-zinc kirimo ingano nto y'ibati kugira ngo cyongere imbaraga n'ubudahangarwa mu gusuka ibintu. Ni amahitamo meza iyo imiterere ikomeye ya bronze nke idakenewe. Muri rusange, aside borax-boric irakenewe iyo ukoresheje iki gicuruzwa.

Isomo rya AWS: RBCuZn-A Icyemezo: AWS A5.8/A5.8M: 2011
Aloyi: RBCuZn-A ASME SFA A5.8

 

Umwanya wo gushushanya: H, V Urusobe rw'ibikoresho byo gutwika:
1330-1550⁰F

 

Ingufu zo Gukurura, kpsi: 50
Uburebure %, ubugari: 30

 

Aho gushonga 1650⁰F Gukomera 1610⁰F Ubukomere bwa Brinell 70-90

Ubuhanga busanzwe bw'insinga nk'uko bivugwa muri AWS A5.8 (agaciro kamwe ni ntarengwa)

Cu Zn Sn Pb Al Ibindi
57.0-61.0 Rem 0.25-1.00 0.05 0.01 0.50

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka irenga 20 dukora electrodes zo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 

 

 

 


  • Ibanjirije iyi:
  • Ibikurikira: