Inkoni yo gusudira AWS A5.11 ENiCrFe-3 Electrodes zo gusudira zishingiye kuri Nickel, Inkoni zo gusudira za Nickel Arc

Ibisobanuro bigufi:

Ni307-3 (AWS ENiCrFe-3) ni electrode ishingiye kuri nikeli ifite sodium nkeya ya hydrogen. Koresha DCEP (electrode ifite umuyoboro w'amashanyarazi ugororotse).


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira ya Nickel na Nickel

Ni307-3                                                     

GB/T ENi6182

AWS A5.11 ENiCrFe-3

Ibisobanuro: Ni307-3 ninikeliElectrode ishingiye ku irangi rifite sodium nkeya ya hydrogen. Koresha DCEP (electrode ifite umuyoboro w'amashanyarazi ugororotse). Ifite ubudahangarwa bwiza bwo gucika kuko irangi ririmo ingano runaka ya manganese, niobium, n'ibindi bintu bivangavanze.

Ikoreshwa: Ikoreshwa mu gusudiranikeli-chromium-icyuma gikozwe mu cyuma (nka UNS N06600) n'ubuso bw'icyuma. Ubushyuhe bwo gukora muri rusange ntiburenze 480 ° C, kandi ubushobozi bwo gucikamo ibice ni bwiza. Bikwiriye gukoreshwa mu gusudira ibikoresho by'umuriro bya atome no mu byuma bikoresha imiti.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Fe

P

S

Si

Cu

≤0.10

5.0 ~ 10.0

≤10.0

≤0.020

≤0.015

≤1.0

≤0.5

Ni

Ti

Mo

Nb

Ta

Ibindi

 

≥60.0

≤1.0

13.0 ~ 17.0

1.0 ~ 3.5

≤0.30

≤0.50

 

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Yemejwe

≥550

≥360

≥27

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

60 ~ 90

80 ~ 100

110 ~ 150

130 ~ 180

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 300°C mbere yo gusudira;

2. Ni ngombwa gusukura ingese, amavuta, amazi n'imyanda ku bice byo gusudira mbere yo gusudira. Gerageza gukoresha agace gato ko gusudira.

 