AWS A5.11 ENiCrFe-9 Ama-electrode yo gusudira ya Nickel na Nickel, Ama-electrode ya Arc y'icyuma yakoreshejwe mu manual, Inkoni zo gusudira

Ibisobanuro bigufi:

Ni327 (AWS ENiCrFe-9) ni electrode ishingiye kuri nikeli ifite sodium nkeya ikoreshwa mu gusiga. Koresha DCEP (electrode ifite umuyoboro w'amashanyarazi ugororotse).


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira ya Nickel na Nickel

Ni327                                                     

GB/T ENi6094

AWS A5.11 ENiCrFe-9

Ibisobanuro: Ni327 ni electrode ishingiye kuri nikeli ifite irangi rike rya sodium. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse)nziza). Icyuma cyashyizwemo gifite ubushobozi bwo kudacika neza kuko icyo cyuma gikozwemo gifite ingano runaka y'ibintu bivangavanze nka molybdenum na niobium.

Ikoreshwa: Ikoreshwa mu gusudira aloyi za nikeli zisaba kudashyuha no kudahura n'ingufu, kandi ishobora no gukoreshwa mu gusudira no gushyira hejuru y'aloyi zimwe na zimwe zigoye gusudira n'ibyuma bitandukanye.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Fe

Si

Cu

Ni

Cr

≤0.15

1.0 ~ 4.5

≤12.0

≤0.8

≤0.5

≥55.0

12.0 ~ 17.0

Nb + Ta

Mo

W

S

P

Ibindi

 

0.5 ~ 3.0

2.5 ~ 5.5

≤1.5

≤0.015

≤0.020

≤0.50

 

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Yemejwe

≥650

≥360

≥18

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

3.2

4.0

Umuyoboro wo gusudira

(A)

90 ~ 110

110 ~ 150

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 300°C mbere yo gusudira;

2. Ni ngombwa gusukura ingese, amavuta, amazi n'imyanda ku bice byo gusudira mbere yo gusudira.

 


  • Ibanjirije iyi:
  • Ibikurikira: