AWS ENiCu-7 Nickel Alloy Welding Rods Ni70Cu30 Nickel Based Welding Electrodes Manual Metal Arc Electrodes

Ibisobanuro bigufi:

Ni202 (AWS ENiCu-7) ni electrode ya Ni70Cu30 Monel alloy ifite titanium calcium coating. Ishobora gukoreshwa haba kuri AC na DC.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira ya Nickel na Nickel

Ni202                                                     

GB/T ENi4060

AWS A5.11 ENiCu-7

Ibisobanuro: Ni202 ni electrode ya Ni70Cu30 Monel alloy ifite titanium calcium coating. Ishobora gukoreshwa haba kuri AC na DC. Icyuma cyashyizwemo gifite ubushobozi bwo kudacika neza bitewe n'ingano ikwiye ya manganese na niobium. Ifite ubushobozi bwo gusudira neza hamwe n'umuriro uhoraho, itaka rito, irakuramo ibintu byoroshye, kandi irasudira neza.

Imikoreshereze: Ikoreshwa mu gusudira aloyi ya nikeli n'umuringa n'ibyuma bitandukanye, kandi ishobora no gukoreshwa nk'ibikoresho byo gupfuka.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Fe

Si

Nb

Al

Ti

Cu

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤2.5

≤1.0

≤1.0

27.0 ~ 34.0

≥62.0

≤0.015

≤0.020

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Yemejwe

≥480

≥200

≥27

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.5

3.2

4.0

Umuyoboro wo gusudira

(A)

50 ~ 80

90 ~ 110

110 ~ 150

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 250°C mbere yo gusudira;

2. Ni ngombwa gusukura ingese, amavuta, amazi n'imyanda ku bice byo gusudira mbere yo gusudira.

 