Tyue Brand Best Arc Welding Electrodes AWS ENiCrFe-1 Nickel Welding Rod, Inkoni yo Gusudira

Ibisobanuro bigufi:

Ni307-1 (AWS ENiCrFe-1) ni electrode ishingiye kuri nikeli ifite irangi rike rya hydrogen sodium. Koresha DCEP (electrode ifite umuyoboro w'amashanyarazi ugororotse).


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira ya Nickel na Nickel

Ni307-1                                                     

GB/T ENi6062

AWS A5.11 ENiCrFe-1

Ibisobanuro: Ni307-1 ni electrode ishingiye kuri nikeli ifite irangi rike rya hydrogen sodium. Koresha DCEP (electrode ifite amashanyarazi adahindagurika). Kubera ko irangi ririmo Nb, icyuma cyashyizwemo gifite plasticity nziza kandi kidacika.

Ikoreshwa: Ikoreshwa mu gusudira aloyi za nickel-chromium-fer (nka UNS N06600, UNS N06601) no hejuru y'icyuma. Ifite ubushobozi bwo gusudira ibyuma butandukanye. Ishobora kandi gukoreshwa ku bushyuhe bw'akazi bwa 980°C, ariko iyo ubushyuhe buri hejuru ya 820°C, imbaraga n'ubudahangarwa bw'umwuka bizagabanuka.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Fe

Si

Cu

Ni

Cr

Nb + Ta

S

P

Ibindi

≤0.08

≤3.5

≤11.0

≤0.8

≤0.5

≥62.0

13.0 ~ 17.0

0.5 ~ 4.0

≤0.015

≤0.020

≤0.50

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Yemejwe

≥550

≥360

≥27

 

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

60 ~ 90

80 ~ 110

110 ~ 150

130 ~ 180

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 300°C mbere yo gusudira;

2. Ni ngombwa gusukura ingese, amavuta, amazi n'imyanda ku bice byo gusudira mbere yo gusudira. Gerageza gukoresha agace gato ko gusudira.

 

 


  • Ibanjirije iyi:
  • Ibikurikira: