ZELLER D350 (UTP DUR 350) ELECTRODE IFITE UBWIYUMVIRO BW'IMYENDA

Ibisobanuro bigufi:

UTP DUR 350 ikwiriye cyane cyane ubuso budashobora kwangirika ku bice bya MnCrV byakozwemo irangi.

Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gushyira mu byiciro
DIN 8555/EN 14700
E1-UM-350/E Fe1
Ibiranga n'aho ikoreshwa
UTP DUR 350 ikwiriye cyane cyane ku bintu birwanya kwangirika ku bice bya MnCrV, nka
Ibikeri, imigozi yo ku muhanda, imigozi yo gushyigikira iminyururu, amapine ya sprocket, imigozi yo kuyobora n'ibindi. Amafaranga asigaye aracyari
ikoreshwa mu gucuranga hakoreshejwe ibikoresho bya karubide ya tungsten.
UTP DUR 350 ifite ubushobozi bwo guhangana n'ingufu zo gukanda no guhindagurika neza iyo ivanze
hamwe n'ubusatsi buke. Icyuma cyo gusudira gishobora gukoreshwa hakoreshejwe ibikoresho bya karubide ya tungsten.
Ubukomere bw'aho amazi acukurwa mu cyuma cyoroshye cyo gusukamo amazi hafi 370 HB
Urwego 1 ku cyuma gifite C = 0.5% hafi 420 HB
Isesengura risanzwe muri %
C Si Mn Cr Fe
0.2 1.2 1.4 1.8 Kuringaniza

  • Ibanjirije iyi:
  • Ibikurikira: