E308-16 electrode yo gusudira icyuma kidafunze

Ibisobanuro bigufi:

Electrode yo gusudira mu byuma bitagira umwandaE308-16 ni electrode yo gusudira yo mu bwoko bwa titaniyumu ikoreshwa mu byuma bidakoresha karubone nyinshi.


  • :
  • Ibisobanuro birambuye ku gicuruzwa

    Ibirango by'ibicuruzwa

    AWS:SFA 5.4 E308-16 Electrode yo gusudira mu byuma bitagira umwanda

    E308-16 ni ubwoko bwa titaniyumuelectrode yo gusudiraku byuma bidakoresha karubone nke cyane.

    Ishyirwa mu byiciro:

    AWS A5.4 / ASME SFA5.4 E308-16

    JIS Z3221 D308-16

    Ibisobanuro:

    Electrode yo gusudira ikozwe mu byuma bitagira umugese E308-16 ni ubwoko bwa titaniyumuelectrode yo gusudiraku byuma bidashonga cyane bifite karuboni nkeya. Icyuma cyo gusudira gifite imiterere myiza ya mekanike kandi kigaragaza ubudahangarwa bwiza na ingese hagati y’udusimba bitewe n’uko karuboni irimo ari ≤. 0.04% b. Gishobora gukoreshwa mu gusudira ahantu hose hamwe n’imikorere myiza: umurambararo uhamye, uduce duto, imiterere myiza ya solder. Kandi na electrode yo gusudira igaragaza imiterere myiza yo kwirinda ubushyuhe, ntibyoroshye guhindura umutuku kandi nta myenge ya gaze ikorwa.

    Porogaramu:

    Gusudira by'icyuma cya 18%Cr-8%Ni.

    Ikwiriye inyubako zo gusudira zakozwe mu cyuma kitagira umukungugu cya 022Cr-19Ni10, nk'imigozi y'ubukorikori, ifumbire,

    ibikoresho bya peteroli, nibindi.

     

    Ibigize imiti mu byuma byabitswe (E308L-16) (%)

    Ikintu C Mn Si Cr Ni S P Cu Mo
    agaciro gasanzwe ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
    Agaciro k'urugero 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

    Imiterere ya tekiniki y'ibyuma byabitswe (%)

    Imikorere yo kurwanya ingese n'imiterere ya ferrite bigomba kugenwa hagati y'umuguzi n'umugurisha.

    Ikintu Imbaraga zo Gukurura (MPa) Uburebure (%)
    agaciro gasanzwe ≥550 ≥25
    Agaciro k'urugero 601 41

    Porogaramu

    Ikoreshwa mu gusudira ubwoko bumwe bw'ibyuma bitagira ubushyuhe birwanya ubushyuhe bikora mu bushyuhe bwinshi, ishobora kandi gukoreshwa mu gusudira icyuma kinini cya chrome gishyuha cyane (nka Cr15Mo, Cr9Mo, Cr13, Cr28) n'ibyuma bitandukanye.

    Ingano (mm)

    2.0

    2.5

    3.2

    4.0

    5.0

    Umuyoboro wo gusudira (A)

    25-50

    50-80

    80-110

    110-160

    160-200

    Ingufu zikoreshwa: AC cyangwa DC+

    Ibisobanuro ku ikoreshwa:

    1. Komeza umugozi ube mugufi uko bishoboka kose.

    2. Kuraho imyanda nk'amavuta n'umukungugu mu mwobo.

    3. Shyira electrodes kuri dogere 350 (662) mu gihe cy'iminota 60 mbere yo kuyikoresha

     


  • Ibanjirije iyi:
  • Ibikurikira: