Amashanyarazi make yo gusudira Electrode AWS E9016-D1

Ibisobanuro bigufi:

J606 (AWS E9016-D1) ni electrode ya elegitoronike nkeya-ikomeye cyane hamwe na potasiyumu ya hydrogène nkeya.Irashobora gukoreshwa kumwanya wose wo gusudira hamwe na AC na DC.Imikorere itajegajega ya AC gusudira iruta iy'ubudozi bwa DC.


Ibicuruzwa birambuye

Ibicuruzwa

Amashanyarazi make yo gusudira Electrode

J606                                       

GB / T E6016-D1

AWS E9016-D1 

 

Ibisobanuro: J606 nigikoresho gito-gifite imbaraga nyinshi zicyuma cya electrode hamwe na potasiyumu ya hydrogène nkeya.Irashobora gukoreshwa kumwanya wose wo gusudira hamwe na AC na DC.Imikorere itajegajega ya AC gusudira iruta iy'ubudozi bwa DC. 

Gushyira mu bikorwa: Byakoreshejwe mu gusudira ibyuma biciriritse biciriritse hamwe nimbaraga nke-zifite imbaraga zingirakamaro zicyuma, nka Q420, nibindi.

 

Ibigize imiti yicyuma (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

60.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Agaciro k'ingaruka (J)

-30 ℃

Bijejwe

90590

90490

≥15

≥27

Yageragejwe

620 ~ 680

00500

20 ~ 28

≥27

 

Diffusion hydrogène yibikoresho byabitswe: ≤4.0mL / 100g (uburyo bwa glycerine)

Igenzura rya X-ray: I amanota

 

Icyifuzo kigezweho:

(Mm)

Diameter

2.0

2.5

3.2

4.0

5.0

5.8

A)

Kuzenguruka

40 ~ 70

70 ~ 90

90 ~ 120

140 ~ 180

180 ~ 220

210 ~ 260

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha 1 kuri 350 ℃ mbere yo gusudira;

2. Ni ngombwa guhanagura ingese, igipimo cyamavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira;

3. Koresha ibikorwa bigufi arc mugihe cyo gusudira.Inzira ifunganye yo gusudira irakwiriye;

4. Iyo igice cyo gusudira ari kinini, kigomba gushyuha hejuru ya 150 ° C hanyuma kigakonja buhoro nyuma yo gusudira.

 




  • Mbere:
  • Ibikurikira: