Ibisobanuro bigufi:

Inkoni zo gusudira AWS A5.1 E6013 (J421) irakwiriye gusudira ibyuma bito bito bya karubone, cyane cyane mu gusudira ibyuma bito bito hamwe no gusudira bigufi kandi bigasabwa kunyuramo neza.


Ibicuruzwa birambuye

Ibicuruzwa

Inkoni zo gusudira AWS A5.1 E6013 (J421) irakwiriye gusudira ibyuma bito bito bya karubone, cyane cyane mu gusudira ibyuma bito bito hamwe no gusudira bigufi kandi bigasabwa kunyuramo neza.

Ibyiciro:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB / T 5117 E4313

Ibiranga:

AWS A5.1 E6013 (J421) ni electrode yo mu bwoko bwa rutile.Urashobora gusudira byombi ingufu za AC & DC kandi birashobora kuba kumwanya wose.Ifite imikorere myiza yo gusudira nka arc ihamye, spatter nkeya, gukuraho slag byoroshye hamwe nubutegetsi-bushobozi nibindi nibindi.Ubushobozi buhebuje-ikiraro hamwe nubushobozi bwa arc.Kubikoresho byo gusudira no gupakira bikwiranye.Intego rusange yinganda nubucuruzi, guteranya no gusudira.

Icyitonderwa:

Muri rusange, ntukeneye kongera gukama electrode mbere yo gusudira.Iyo yibasiwe nigitonyanga, igomba kongera kuyumisha kuri 150 ℃ -170 ℃ kumasaha 0.5-1.

Umwanya wo gusudira:

PA, PB, PC, PD, PE, PF

AWS A5.1 E.

Ibigize imiti yibikoresho byose byasudutse: (%)

Ibigize imiti

C

Mn

Si

S

P

Ni

Cr

Mo

V

Ibisabwa

≤0.10

0.32-0.55

≤0.30

≤0.030

≤0.035

≤0.30

≤0.20

≤0.30

.080.08

Ibisubizo bisanzwe

0.08

0.37

0.18

0.020

0.025

0.030

0.035

0.005

0.004

Ibikoresho bya tekinike yububiko bwabitswe

Ikizamini

Rm (N / mm2)

Rel (N / mm2)

A (%)

KV2 (J) 0 ℃

Ibisabwa

440-560

≥355

≥22

≥47

Ibisubizo bisanzwe

500

430

27

80

Reba Ibiriho (DC)

Diameter

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40 ~ 70

50 ~ 90

80 ~ 130

150 ~ 210

180 ~ 240

Igenzura rya X-Ray:

Urwego Ⅱ