AWS E7015 Inkoni yo gusudira

Ibisobanuro bigufi:

AWS A5.1 E7015 ni sodium ya hydrogène nkeya yubatswe na karubone ibyuma bya electrode.


Ibicuruzwa birambuye

Ibicuruzwa

AWS A5.1 E7015 ni sodium ya hydrogène nkeya yubatswe na karubone ibyuma bya electrode.

E7015 gusudira electrode igomba gukoreshwa kuri DCEP.Ifite imikoreshereze myiza yo gusudira ituma ishobora gukora imyanya yose yo gusudira, ifite arc ihamye, gukuraho slag biroroshye kandi ifite spatter nkeya.Icyuma cyabitswe gifite imikorere yubukanishi no kurwanya-gukanura, bitanga ubushyuhe buke bwo hasi.

Gusaba

AWS A5.1 E. ibyuma bya karubone bigoye gusudira.

Hindura kuri Standard

GB / T 5117 E5015

AWS A5.1 E7015

ISO 2560-BE 49 15 A.

Intego: AWS A5.1 E7015 ikoreshwa mugusudira ibyuma biciriritse bya karubone hamwe nububiko buke buke nka 16Mn, 09Mn2Si, 09Mn2V hamwe nicyuma gikoreshwa mubwubatsi bwubwato nka A, B, D, E. Irakoreshwa kandi mubyuma byimbitse amasahani hamwe nicyuma cya karubone bigoye gusudira.

Ibigize imiti (%)

Ibigize imiti

C

Mn

Si

S

P

Ni

Cr

Mo

V

Agaciro k'ingwate

≤

0.15

≤

1.60

≤

0.90

≤0.035

≤0.035

≤

0.30

≤

0.20

≤

0.30

≤

0.08

Igisubizo rusange

0.082

1.10

0.58

0.012

0.021

0.011

0.028

0.007

0.016

Ibikoresho bya tekinike yububiko bwabitswe (Shielding Gas: CO2)

Ikizamini

Rm (MPa)

ReL (MPa)

A (%)

KV2 (J)

-20 ℃ -30 ℃

Agaciro k'ingwate

90490

00400

≥20

≥47

≥27

Igisubizo rusange

550

450

32

150

142

X-Ray Radio-ibishushanyo bisabwa Ibizamini: Icyiciro I.

Reba Ibiriho (DC +)

Diameter (mm)

Φ2.5

Φ3.2

Φ4.0

Φ5.0

Amperage (A)

60 ~ 100

80 ~ 140

110 ~ 210

160 ~ 230

Inyandiko:

1. Electrode igomba gushyuha kubushyuhe bwa 350 ° C kumasaha 1.Shyushya inkoni igihe cyose ikoreshejwe.

2. Umwanda nk'ingese, irangi ry'amavuta hamwe n'ubushuhe bigomba guhanagurwa ku gice cy'akazi.

3. Arc ngufi irasabwa gukora gusudira.Inzira nini yo gusudira irahitamo.


  • Mbere:
  • Ibikurikira: